Saravanan Sornam <sarava...@gmail.com>
Sent by: material...@googlegroups.com 02/11/2015 03:09 PM
|
|
--
You received this message because you are subscribed to the Google Groups
"Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send
an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkJTi2HFtthS5J5c7_DX9Nkw%3DrtUL0As75iEfmSdnqKepg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
----------------------------------------------------------------------------------------------------------
Information transmitted by this E-MAIL is intended only for the use of the addressee(s) and contains information that is privileged, confidential or exempt from disclosure under applicable law. If you are not the intended recipient or it appears that this mail has been forwarded to you without proper authority, you are notified that any use or dissemination and or copying of this email in any manner is strictly prohibited and you are requested to delete this e-mail immediately.
Communicating through e-mail is not secure and capable of interception and delays. Any one communicating with TATA Consulting Engineers Ltd., and / or its subsidiaries or associates or group companies by e-mail accepts the risks involved and their consequences.
While this e-mail has been checked for all known viruses, the addressee should also scan for viruses and notify the originator of e-mail.
---------------------------------------------------------------------------------------------------------
Hi joshi,
Please send any reply through the group mail id.
As per ASME Sec IX, QW 422 table, SA 182 F 92 is given, its P no. is 15E.
From design point of view, what is the equivalent forging can be used with the same allowable stress.
Regards
Saravanan