Dear Experts 

 Can i proceed forming of 30 mm thk Plate by joining of 2 Plates for  Lower shell dish end.

If cant what would be the acceptable of joining length of plates.
If yes what precaution to be take care.

Any reviews 

can any one help me 

Regards
chaitanya kamal 
ph-8226081506  



Dish end.pdf

Vishwas Keskar

unread,
Jul 15, 2022, 2:13:18 AM7/15/22
to material...@googlegroups.com
 Hope this is Carbon steel dished end.
First discuss with Design Engineering about this  chordal joint in dished end.
Then locate the joint based on plate width.
Get the drawing.
Check with Dished end forming expert , Is this dished end is  cold forming or hot forming. 
Based on forming Method,  select WPS.
Finalise proposal in consultation with 
Methods Engineering, Design Engineering,  QA and Manufacturing. 
Accor. prepare QAP  Method statement  and circulate to Mfg as per ISO issue document 

Vishwas 
IWE -
International Welding Engineer



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/57bd9e9a-da16-4e1c-ba2b-dc806d01205bn%40googlegroups.com.

Anilkumar G

unread,
Jul 15, 2022, 3:31:16 AM7/15/22
to material...@googlegroups.com
Yes you can. Consult with your design team for this.
Weld according to a qualified WPS.
You may need RT for the full length joint after forming and after heat treatment if applicable.

Regards
Anilkumar

madheswaran s

unread,
Jul 16, 2022, 9:04:49 AM7/16/22
to material...@googlegroups.com
Dear All, I have one doubt, 

in wps there is a line Pulsing current --------in the format. If i prepare new wps , what to write there -- if I process SMAW? IF process GTAW, IF process SAW, IF process GMAW? can i one tell for each process.

Sankaran Sp

unread,
Jul 17, 2022, 12:50:18 AM7/17/22
to material...@googlegroups.com
Dear Mr.Matheswaran,

Find the reply for your questions:

pulse current is applicable to GATW & GMAW only not for SMAW & SAW process.
type of current - AC or DC with pulse or without pulse 
typr of polarity : DCEP or DCEN

Regards,
Sankaran.SP
Coimbatore, India. 