Regarding Welding of 0.5 & 0.8 mm thk sheet

24 views
Skip to first unread message

Mohit Aggarwal

unread,
May 18, 2016, 8:27:30 AM5/18/16
to materials-welding

Dear Experts,

We are doing manual TIG Welding of cassette to cassette of thk 0.5mm and 0.8mm. But material is not get fused properly at various locations.

Here is the attached photo.

Kindly suggest the procedure for improvements.

Best Regards,
Mohit Aggarwal.
+919619549616

IMG_20160517_150000.jpg
IMG_20160517_145949.jpg

Mohd Siraj

unread,
May 21, 2016, 11:00:27 PM5/21/16
to Materials & Welding
Hope it is autogeneous weld.

Increase little weld current slower speed and good clamping.