We have straighten the pipe material SA234 WP9, PNo. P5B, for qualification of procedure.Now we will have to done Normalizing and tempering of plate welded material.

Kindly suggest at what temperature we should done the Normalizing 

Also let me.konw is there any post heating requirements are there for this material.or not.

Material is SA234WP9 20mm thk drawn  from.pipe into plate hardness is 190 BHN after straightening and cutting processes.

Best Regards,
Mohit Aggarwal.
9821958461

Kannayeram Gnanapandithan

unread,
Apr 2, 2017, 3:16:54 AM4/2/17
to materials-welding
With welding?.For base check with MTC

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPOyDC%3Dcwyv9GWzU_VrZMA9vj_nKKSA1un_V1ws9nBhKPQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Mohit Aggarwal

unread,
Apr 2, 2017, 7:30:42 AM4/2/17
to materials-welding
Dear Sir,

Yes with Welding we are joining to qualify procedure so that we can used it for welded fittings..

Kannayeram Gnanapandithan

unread,
Apr 5, 2017, 4:50:38 AM4/5/17
to materials-welding
what is classification of welding rod

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Sun, Apr 2, 2017 at 2:35 PM, Mohit Aggarwal <aggarwa...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (aggarwa...@gmail.com) Add cleanup rule | More info

Dear Sir,

Yes with Welding we are joining to qualify procedure so that we can used it for welded fittings..
On Apr 2, 2017 12:46 PM, "Kannayeram Gnanapandithan" <kgpan...@gmail.com> wrote:

For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.

Mohit Aggarwal

unread,
Apr 5, 2017, 8:04:38 AM4/5/17
to materials-welding

George Dilintas

unread,
Apr 5, 2017, 8:16:42 AM4/5/17
to Meghanadh K
Normalizing is usually done at 900degC with subsequent cooling on still air

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALTezPOyDC%3Dcwyv9GWzU_VrZMA9vj_nKKSA1un_V1ws9nBhKPQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

Mohit Aggarwal

unread,
Apr 6, 2017, 12:48:37 AM4/6/17
to materials-welding
We have mentioned it in 1020 dega -1040 deg C 
And posheating has done for 3.5 hours for P9 

Ankit Gandhi

unread,
Apr 12, 2017, 2:06:00 AM4/12/17
to Materials & Welding, pgos...@quickclic.net
For Normalizing & tempering you should follow Material Test certificate, 
If i am not wrong then you want Elbow from Plate material, so you have to check for fiber elogation also.
As per requirement of fiber elongation you need stress reliving same weld joint also followed in PQR.
Hope this can help you.

Ankit Gandhi
8879457665