Respected Experts,
Greetings!!
Attached here with photo of SS316L weldolet on Pipe of 10" 4 thk of SS316L.
After Welding pipe distort towards inside as shown.
Kindly suggest the remedy and technique to control further distortion.
Best Regards,
Mohit Aggarwal.
Welding Engineer.
we have cool down the weld in between.
How we can cool in more effective way??
weldolet welding.
Its seems u hd continuos welding without properly cooldown weld.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e63eb1d3-7443-48ea-a1eb-6d62d8ba69c7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
| From: Mohit Aggarwal Sent: Δευτέρα, 4 Ιουλίου 2016 - 04:19 To: materials-welding Reply To: material...@googlegroups.com Subject: Re: [MW:25058] Regarding distortion control. |