6.2.2(d)is for war not for wps
On Sun 22 Apr, 2018 8:17 am 'ramen samanta' via Materials & Welding, <materials-welding@googlegroups.com> wrote:
Dear JoydevPl. ref. API- 1104- clause 6.2.2 (d)- dia. groupsThanks,R.K.Samanta
Dear Expert,--Please suggest Dia range.for WPS as per API 1104.--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Hi
API 1104 covers welding procedures qualifications as below,
Case
1. Clause 5 Welds Containing Filler-metal Additives
2. Clause 12 Mechanized Welding with Filler Metal Additions
3. Clause 13 Automatic Welding Without Filler metal Additions
Diameter range is not essential for case 1 WPS/PQR, i.e. 5.3.2.3 however “the ranges of outside diameters and wall thicknesses over which the procedure is applicable shall be identified”.
Means unlike ASME sec 9, WPS/PQR format, additionally you may need to specify the restriction on outside diameter and thickness in order to facilitate to have control on welders use in production welding ( based on clause 6.2.2 d )
Diameter range for case 2 & 3 WPS/PQR is essential variable, refer respective clauses - 12.5.2.5 & 13.5.2
Also refer API 1104 interpretation ( specifically Page 82 /94 ) attached herewith for more details. There are many questions based on this topic only.
Downloaded from
http://mycommittees.api.org/standards/techinterp/transpipe/default.aspx
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c23d7c90-1f2b-4a58-ab4d-651cbde1c374n%40googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB7ASHfYfxE5EueVm%3D-RXgMmD%2BY5m9rOPbwAU9q0V9tMRFYhOw%40mail.gmail.com.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c23d7c90-1f2b-4a58-ab4d-651cbde1c374n%40googlegroups.com.
With Regards Vijay Kumar Konathala |
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1905163163.1958475.1603399320543%40mail.yahoo.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BQ29OiC63ssUfxaB3dAga2Oug9mkQ%2B2qXfHPwv9C1zxo%3Doqnw%40mail.gmail.com.