The Primary supports are welded to pipe ( Carbon steel) and PWHT was not done for amine service.  All the butt welds have undergone PWHT.  PWHT issue was noticed after completion of commissioning.  As per API  945, residual stresses are one of the reason for amine cracking.  Please advise how we can convince client  that residual stresses due to pipe supports welding have no effect on amine cracking.

Ramin Kondori

unread,
Jul 9, 2019, 11:18:08 PM7/9/19
to material...@googlegroups.com
PWHT shall be done.

Ramin  Kondori
Sr. QA/QC & Welding Engineer
-----------------------------------------------------------
PG-Dip. in Welding Engineering (IWE  AT  0070)
BSc. in Civil Engineering (IUT)
BGAS Painting Inspector
ASNT Level I&II
                        
IIW-Logo-Colour-small



On Tue, Jul 9, 2019 at 9:24 AM N VENKATESWARA PRASAD <weldeng...@gmail.com> wrote:
Dear Experts,

The Primary supports are welded to pipe ( Carbon steel) and PWHT was not done for amine service.  All the butt welds have undergone PWHT.  PWHT issue was noticed after completion of commissioning.  As per API  945, residual stresses are one of the reason for amine cracking.  Please advise how we can convince client  that residual stresses due to pipe supports welding have no effect on amine cracking.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL%3D4YYiBmE7g%3DvhJH0xboyNPYi8m%2BpPp%2BY7NbM54APzDaDMCNQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

manish kulkarni

unread,
Jul 9, 2019, 11:18:08 PM7/9/19
to material...@googlegroups.com
Are you convinced that PWHT is not required?
If yes, on what basis against cracking mechanisms?
Regards


On Monday, July 8, 2019, 8:23 PM, N VENKATESWARA PRASAD <weldeng...@gmail.com> wrote:

Dear Experts,

The Primary supports are welded to pipe ( Carbon steel) and PWHT was not done for amine service.  All the butt welds have undergone PWHT.  PWHT issue was noticed after completion of commissioning.  As per API  945, residual stresses are one of the reason for amine cracking.  Please advise how we can convince client  that residual stresses due to pipe supports welding have no effect on amine cracking.

--
Reply all
Reply to author
Forward
0 new messages