Clarification Required

59 views
Skip to first unread message

Madhava Ram

unread,
Mar 17, 2023, 8:25:18 AM3/17/23
to material...@googlegroups.com
Dear Team,
As per ASME Sec IX 2021
IS 2062 E350 is an unassigned grade whish is not listed in the QW/QB_422 but our client is insisting us to add the material in P1 and G2 to perform the PQR and WPS qualification.
Kindly share your option on this

Thanks in Advance
--
With Regards,


Madhavaram E

Tomas gonzalez

unread,
Mar 18, 2023, 1:44:43 AM3/18/23
to material...@googlegroups.com
Not posible to correspond P number to material not included in Section IX.
Only will be qualified for the specific material.

Regards 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPtDbpq5A5%3Dw3hANsL33zZ0gX3_1jWF1JxBiJ1eQGcb4phXPQA%40mail.gmail.com.

Jenish Mistry

unread,
Mar 18, 2023, 5:58:02 AM3/18/23
to material...@googlegroups.com
Dear sir,

Can not use correspond IS 2062 E350 as P1 G2 group because it does not fall in QW 420.

Your procedure qualification should be as per Unassigned Metal to either assigned or Unassigned Group as per QW 424. 
 

--