May I get a clarification about the welders performance Monitoring, is it 
by :Defect Inchs/Total inchs Welded
or by :RT Film Rejected/Total RT Film Taken
or by :Defect Inchs/Total Inchs Examinated with RT

For Information the NDT carried out by other subcontractor.

Is there any of that in standards?

Thanks in advance.

D. Zaidi

Rajendra Jadhav

unread,
Apr 21, 2017, 2:36:02 AM4/21/17
to material...@googlegroups.com
Dear ,

Please refer SEC IX for welder qualification(performance).
For welder qualification you have to maintain weld running sheet including heat input, current, voltage etc.
And NDT part may depend on client requirement.
RT is most common NDT method for welder qualification.

regards,
Rajendra Jadhav

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9dad54ce-1b97-41d1-b203-6312d759df97%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Perumal Govindan

unread,
Apr 21, 2017, 2:36:06 AM4/21/17
to material...@googlegroups.com

Hi

Repair %= No. of repairs/No. of RT films reviewed *100.

Regards
P Govindan

--

MUNHOZ Sergio TECHINT

unread,
Apr 21, 2017, 8:13:24 AM4/21/17
to material...@googlegroups.com

There are different ways to monitor the welding performance, usually you can use:

 

·         For RT: “Number of rejected films” per “Total Number of films”

·         For UT: “Length of defect” per “Total length inspected”

·         For Joints: “Number of Joints repaired” per “Total number of Joints” or “Number of cut of joints” per “Total number of joints”

 

You shall agree the method and the limits acceptable with your client during the bidding stage of the Project once it can involve high control costs.

 

Best regards

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.

Reply all
Reply to author
Forward
0 new messages