need a clarification about NACE & standtard requiremnt -reg

96 views
Skip to first unread message

Sankaran Sp

unread,
Apr 12, 2020, 12:20:32 AM4/12/20
to Materials & Welding
Dear friends,

if we place the order to any steel foundry to supply the casting ( A 216-WCB)  with NACE requirements. while see the casting MTC they use to mention the above casting are meeting the requirements of NACE MR 0175 or MR 0103 requirements
means what? what are the additional activities being followed for NACE castings in foundry than standard casting ? can you any body give me a details.   

Regards,
Sankaran.SP
Welding & Metallurgy expert

james gerald

unread,
Apr 12, 2020, 11:46:46 PM4/12/20
to 'Sankaran Sp' via Materials & Welding
1. Final Heat Treatment condition
2. If Repaired, Qualification of PQR with Hardness requirements & Locations
3. Base Metal Hardness requirements
4. Chemical composition restriction like sulphur and Nickel
5. Based on Purchaser requirement, any HIC or SSC test

Thanks & Regards

J.Gerald Jayakumar



--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1625659408.2218431.1586593902186%40mail.yahoo.com.

TDK YOKESH

unread,
Apr 13, 2020, 12:20:40 AM4/13/20
to material...@googlegroups.com
Dear sir,
Kindly see the requirements specified in Nace MR0175 clause 8. 


chandraknat vaidya

unread,
May 9, 2020, 11:31:55 PM5/9/20
to material...@googlegroups.com
What are the guidelines for selection of Soultion A/B/C when using NACE TM0284 7 0177?
Regards
Chandu