To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3iyrdv9lox8x20ty5lg4u3oy.1441099054584%40email.android.com.
For more options, visit https://groups.google.com/d/optout.
If you have the material Certificate of Compliance from the mill yes.
If you want to verify the material then this should be for your information only.
Be very careful trying to recertify material.
By doing so you could be assuming liability.
Best Regard,
Jim Price | Welding Engineer, CWI
Direct: 320.7463439 |
![]()
From: material...@googlegroups.com [mailto:material...@googlegroups.com]
On Behalf Of Kadir godil
Sent: Tuesday, September 01, 2015 3:55 AM
To: Materials & Welding
Subject: [MW:23378] DN 80 Carbon steel pipe
Dear Experts,
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/6ee1a86223254eaf8696d446166e76ce%40POLARMAIL.PolarTank.local.