it is alternative as per ASME, however need to perform in addition to qualification if DEP is applicable in your project

On Sun, 24 Jul 2022 at 14:21, Sam Raja.A <samr...@gulfspic.com> wrote:

Dear Sir,

 

Is  first production required for already qualified welder/welding operator  as per sec ix qw-304.1/qw305.1?

 

It is mentioned shell dep specification.

 

Kindly advise us any code reference.

 

Thanks & Regards,

Sam Raja

QC Inspector,

Gulf Spic

Kuwait

Mob-+965-65007906

 

TDK YOKESH

unread,
Jul 26, 2022, 6:47:48 AM7/26/22
to material...@googlegroups.com, Sam Raja.A
Refer shell DEP 31.38.01.31 . Also the DEP version applicable to be noted . The requirements has been revised lately. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubkjTdKpwC9BFO%3DZuE9Nd%2Bw09xzweLJ2wyQATXnaronMrQ%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages