Dear all

We have aluminum 5083 tank which have some small hopes in shell plates 
We prefer to go for injection wields to close these hopes 
Holes are in 5 mmm diameter 

Can you advice procedures and electrode to be used?

Regards 
HA

On Mar 17, 2017 3:33 PM, "Hani Al Masry" <hanyo...@gmail.com> wrote:

Dear All

Please advice we have to fabricate some pulling heads from pipes grades 
X60 and X65 with plates grade S355 

We proposed WPS for welding of X65 as the higher grade to be covered also for X60 and for S355 

Is these WPS 's are enough?or we need other?

HA
Regards

Kannayeram Gnanapandithan

ungelesen,
26.04.2017, 06:19:0926.04.17
an materials-welding
5183

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Tue, Apr 25, 2017 at 8:32 PM, Hani Al Masry <hanyo...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (hanyo...@gmail.com) Add cleanup rule | More info
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKOkEzfEQx73UVqQGT98%2BzCXR356MFtQTaWfZNh0NsKv6vQjew%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


Hani Al Masry

ungelesen,
26.04.2017, 06:38:3126.04.17
an material...@googlegroups.com
Yes exactly but it's not available in UAE
I will use instead 5356 1.6mm?
Also what should do to concert the machine to GMAW?
Can you send me WPS?

Regards
H.A

Kannayeram Gnanapandithan

ungelesen,
26.04.2017, 09:04:1826.04.17
an material...@googlegroups.com
Yes,u can,but use He75%+Ar25%. Clean thoroughly while fit up and before start of welding.