FCAW substitude for SMAW in offshore platforms

32 views
Skip to first unread message

EmaD FaRaHanI

unread,
Mar 6, 2021, 6:07:56 AM3/6/21
to material...@googlegroups.com
Dear All,
I want to replace SMAW in the fabrication of offshore platforms, top side section.
In this regard, FCAW is selected mainly for most of the welds, to increase the speed of fabrication.
May I know:
1- Is FCAW the right choice? how about GMAW?
2- In the case of FCAW, which electrode with a 3.2mm size is proper for all position welding in offshore platforms? mainly high strength steels

Regards,
E.F

Chris Sabu

unread,
Mar 6, 2021, 6:29:02 AM3/6/21
to material...@googlegroups.com
E71T1c is a good choice if you were using 7018 in smaw.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABtwbJE2HAz97vDLBZLea6Rd8vjfo64-gngvW4WXMDyiE5Rc-w%40mail.gmail.com.
--
THANKS AND REGARDS
CHRIS SABU
0559695451

Hani Al Masry

unread,
Mar 14, 2021, 11:42:46 PM3/14/21
to material...@googlegroups.com
E71T1 1.2MM WIRE FOR FCAW , however shielded gas is an issue for outdoor welding with FCAW?
You may use 7106-1 for root pass only then complete rall with FCAW 

Regards,
H.A  