WPS compatibility for A36 and S275JR?

313 views
Skip to first unread message

chris

unread,
Apr 18, 2020, 7:32:44 AM4/18/20
to Materials & Welding
hello friends,

I have a WPS with ref code AWS D 1.1 for A36 can I use the same for welding S275JR as well? 
I would like to know if there is any code prohibition for this? Even though the materials are almost the same except for a higher yield strength for S275.


Best regards

Chris

Harish Kannepalli

unread,
Apr 18, 2020, 7:43:18 AM4/18/20
to material...@googlegroups.com
Hi,
  S275JR is unlisted material in AWS D1.1, so you have to make a new WPS.

Regards,
Harish Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3a35de5b-edc0-4d7a-a713-ba7e405c7572%40googlegroups.com.

Maha Charu

unread,
Apr 21, 2020, 1:30:13 AM4/21/20
to material...@googlegroups.com
Make one pre-qualified wps, that all

--

chris

unread,
Apr 21, 2020, 12:35:52 PM4/21/20
to Materials & Welding
thank you. Is there any inclusion in P nos?


On Saturday, April 18, 2020 at 3:43:18 PM UTC+4, Harish wrote:
Hi,
  S275JR is unlisted material in AWS D1.1, so you have to make a new WPS.

Regards,
Harish Kumar

On Sat, 18 Apr 2020, 17:02 chris, <chris...@gmail.com> wrote:
hello friends,

I have a WPS with ref code AWS D 1.1 for A36 can I use the same for welding S275JR as well? 
I would like to know if there is any code prohibition for this? Even though the materials are almost the same except for a higher yield strength for S275.


Best regards

Chris

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to material...@googlegroups.com.

Maha Charu

unread,
Apr 23, 2020, 2:57:07 AM4/23/20
to material...@googlegroups.com
If ur project is Aramco, no need new WPS, Aramco considered both grades are equalent, ref 12-SAmss-7

To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/86dad886-50a4-484f-a072-384c98b711c1%40googlegroups.com.
Reply all
Reply to author
Forward
0 new messages