Dear Experts,
Our piping team prepared the orifice flange nipple seal welding & PT after hydro test
But, our client wants to install the nipple & seal weld before hydro test
Which is the right method?
Regards,
Amul Raj T
Before.
To ensure no leak during hydrotest.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f8a8c0b9-3470-40fc-bd5e-08588cd833c2%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Dear Amul,
Need before hydro.
Arun nair.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/501913ef-9fd0-4f55-8675-d2dfe74a6d0d%40googlegroups.com.
--