Hi Neilashkumar,
There’s no answer to such questions in these “Open Forum”. If such conditions are stipulated in your project specifications, then it’s deemed as mandatory. In order to get a deviation or any waiver please discuss the same with clients and then come up with some consent/understanding.
Many clients insists on “Dehydrogenation” to safeguard against hydrogen induced damages (especially wet hydrogen cracking”) in refining environments. In view of such imminent damage and other forms of hydrogen damages in refining environments, dehydrogenation treatment is most commonly asked for in present day fabrication standards.
Thanks.
Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist &
Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299
Dear All,
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAOT5XfyRhstKvyeqQRSrfFXCgAAAEAAAAN8IATtSA6xDg3KrvkrY%2BRkBAAAAAA%3D%3D%40quickclic.net.
If customer requirements, no other way
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB%3DAs8n_R5gx9-5ayzUu4gDNk8WvpZxhJt8AKAkGQejvRNHW4Q%40mail.gmail.com.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0B59ABE0-AA41-4BD5-9389-F1AF70590CAB%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.