Aluminium Welding

43 views
Skip to first unread message

afrozsh...@gmail.com

unread,
Jan 21, 2016, 7:57:43 AM1/21/16
to Materials & Welding


Dear Expert

It sound very strange , but I got information there is some non - heat treatable aluminum grade of material which can welded without addition of filler wire metal.

Is it true ?

Regards,

Afroz Shaikh

IOTIES

Kannayeram Gnanapandithan

unread,
Jan 21, 2016, 10:25:34 AM1/21/16
to materials-welding

Yes, u can

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2254bac0-f641-47a3-92ef-cb3c116598ef%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

ahmed

unread,
Jan 21, 2016, 10:06:21 PM1/21/16
to material...@googlegroups.com

Yes, there are non-heat treatable aluminum alloys.

Maulik Thakkar

unread,
Jan 21, 2016, 11:10:02 PM1/21/16
to Materials & Welding

Dear sir,

Welding of aluminium without addition of alloying element is not recommended due loss of alloying elements in final weld. If total alloying elements reaching < 4% then weld may crack.

Refer curve: Effect of alloying additions on crack sensitivity of aluminium alloys.

--
Reply all
Reply to author
Forward
0 new messages