Ti B effect impact value

6 views
Skip to first unread message

Pravin Poornachandran

unread,
Feb 10, 2017, 1:58:15 AM2/10/17
to 'Bijay' via Materials & Welding
Dear expert, 

I would like to know what is the relation between Ti-B and impact value. Addition or reduction of this 2 elements would affect the impact value? 

Seeking for expert advice. 

Best regards, 
Pravin Poornachandran

Kannayeram Gnanapandithan

unread,
Feb 11, 2017, 1:59:21 AM2/11/17
to materials-welding
B will increase Hardness

THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Fri, Feb 10, 2017 at 8:45 AM, Pravin Poornachandran <htcis...@gmail.com> wrote:
Boxbe This message is eligible for Automatic Cleanup! (htcis...@gmail.com) Add cleanup rule | More info
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADDyn7d2MFWyE3wcMMmOAigmN0rB4Er3baEtwK8zx89hT%2BNNzw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.


Reply all
Reply to author
Forward
0 new messages