Thickness Qualification Range of Impact tested WPS for Piping

117 views
Skip to first unread message

Biplab Pal

unread,
Jan 12, 2016, 3:40:35 AM1/12/16
to materials-welding
Dear Experts,

If impact test is required for any WPS the base metal thickness limit is an supplemental material and qualification of minimum thickness limit shall follow QW-403.6.
Now our Consulting Service Department is telling us the qualification thickness limit shall be t/2 to t+6mm. as per ASME B 31.3 table 323.3.1 for piping.

Guys, did you faced this kind of problem? I am experiencing this problem 1st time.
Please let me know your understanding and experience.

--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

george....@gr.bureauveritas.com

unread,
Jan 15, 2016, 8:49:01 PM1/15/16
to material...@googlegroups.com

Indeed there the requirement of B31.3 is different

best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


Inactive hide details for "'Biplab Pal' via Materials & Welding" ---12/01/2016 10:40:52---Dear Experts, If impact test is requi"'Biplab Pal' via Materials & Welding" ---12/01/2016 10:40:52---Dear Experts, If impact test is required for any WPS the base metal thickness limit is an

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-weld...@googlegroups.com.
To post to this group, send email to
material...@googlegroups.com.
Visit this group at
https://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/CAFnzQg0dM%3D3Ds_S16LGd30N5qLYbfMKHhkM-9riQpzgRpAQGkw%40mail.gmail.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

Kannayeram Gnanapandithan

unread,
Jan 15, 2016, 8:51:16 PM1/15/16
to materials-welding

Ur client is ok

--

Biplab Pal

unread,
Jan 15, 2016, 11:19:47 PM1/15/16
to materials-welding

Raghuram Bathula

unread,
Jan 15, 2016, 11:22:20 PM1/15/16
to Materials-Welding
yes construction code (B31.3) limits will apply

Vino Varghese

unread,
Jan 16, 2016, 10:43:03 AM1/16/16
to material...@googlegroups.com

One has to refer the applicable Construction Code for the Impact test requirement. If its, ASME B31.3, you need to follow the same.

Regards, Vino

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.

afrozsh...@gmail.com

unread,
Jan 19, 2016, 8:30:48 AM1/19/16
to Materials & Welding

Dear Biplab,

As QW403.6 & ASME  B 31.3, thickness qualification range will be as mentioned below

Minimum Thickness qualification :(1) If t is more than 6 mm then  min thickness qualifies will be  t or 16 mm whichever is less (2)If t is less than 6 mm then min thickness qualifies will be 1/2 t
 
Max Thickness Qualification: t + 6 mm

Regards,

Afroz Shaikh
IOTIES

Biplab Pal

unread,
Jan 20, 2016, 4:44:08 AM1/20/16
to materials-welding, pradip....@gmail.com
Dear all,

1st thanks for your kind support.

So we are in conclusion of 2 as all people suggested.
As per ASME B 31.3 if we are qualifying a WPS the following shall apply.

Case 1. If thickness of test piece is less than 6mm then qualification range will be 1/2t to t+6.
    If thickness of test piece is above 6mm then qualification range will be either 16 or t to t+6.

Case 2. for all 1/2t to t+6.


Please provide your input which one is correct case 1 or case 2 ??


Thanks & Regards



For more options, visit https://groups.google.com/d/optout.



--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   bipla...@gmail.com
 
Reply all
Reply to author
Forward
0 new messages