Thanks & Regards
J.Gerald Jayakumar
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/361481876.3065893.1586752043677%40mail.yahoo.com.
our customer specifies ultra low carbon content with elevated nickel. Is there any other welding that i can use in this case?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f52cfb16-c52a-436a-a0af-7437a3aa51c8%40googlegroups.com.

Thanks & Regards
J.Gerald Jayakumar
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1247802736.3267726.1586791298688%40mail.yahoo.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1247802736.3267726.1586791298688%40mail.yahoo.com.