QT stamp on Quenched and Tempered forgings

39 views
Skip to first unread message

vivek kb

unread,
Sep 7, 2021, 12:48:10 AM9/7/21
to material...@googlegroups.com
Dear Experts,

Below is an excerpt from ASME SA-350 and is related to product marking:

image.png

Could you please advise the basis of this requirement. In most cases, this stamping is specified for Quenching and tempered or Quenching and precipitation heat treated only unlike the Normalizing or Normalized and tempered.

Regards,
Vivek.

Kannayeram Gnanapandithan

unread,
Sep 7, 2021, 8:26:34 AM9/7/21
to materials-welding
Toughness value will be  more than Normalizing, Welding related issues will be more in QT if proper procedure is not followed. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAB3WdPMJ0Rz4F0ZaRKJiFx_HkZbr%3DpNiOhtqKiMdEM6AA4%3DSwA%40mail.gmail.com.

james gerald

unread,
Sep 9, 2021, 12:11:16 AM9/9/21
to material...@googlegroups.com
Check your MTC for the type of Heat Treatment performed and take necessary action with the concurrence of your Client.

Thanks & Regards

J.Gerald Jayakumar



--