Dear all,

What is the exact defination of ferritic steel as per ASME or ASTM or EN standard.

Kindly clarify

Regards 

Kannayeram Gnanapandithan

nepročitano,
16. velj 2022. 02:30:4916. 02. 2022.
u materials-welding
Less Carbon, High Chrom and some small  addition of alloying elements Nb, Ni etc
U can not hardened by heattreatment

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALi4c7M_Yv5pZ2eRgWjLGTcXPwtBRTM0S5o1idRkeMAmidU-TA%40mail.gmail.com.

Jenish Mistry

nepročitano,
16. velj 2022. 22:22:0916. 02. 2022.
u material...@googlegroups.com
Dear sir,

Why it can not hardened by heat treatment?

By which process it can hardened ??




--
Thanks for your best support.

Regards,
Jenish Mistry
09033476117

Vinay

nepročitano,
16. velj 2022. 22:22:1016. 02. 2022.
u material...@googlegroups.com
pl see reply of KG ..Ferritic stainless steel is defined as a  high chromium non-hardenable class of stainless alloys ,which has chromium content up to  to 30% and a carbon below 0.02 %. These steels are essentially non-hardenable by heat treatment .

--

Kannayeram Gnanapandithan

nepročitano,
16. velj 2022. 23:12:1716. 02. 2022.
u materials-welding
misunderstood asFerritic stainless steel.  All carbon, low alloy steel are ferritic steel which can be heat treated

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

SN

nepročitano,
16. velj 2022. 23:35:4916. 02. 2022.
u material...@googlegroups.com
Dear all,

As there any supporting national or international standards available which  exactly spell the definition of feritic steel as client was a reference for the same.

Thanks

Shahil Saini

nepročitano,
17. velj 2022. 00:55:0917. 02. 2022.
u material...@googlegroups.com
Hello SN, 

You can refer to the International- ASM handbook. Please find the attachment

Chapter_1 ASM.pdf

George Dilintas

nepročitano,
22. velj 2022. 23:00:1822. 02. 2022.
u material...@googlegroups.com
ferritic steels can be hardned 



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Odgovori svima
Odgovori autoru
Proslijedi
0 novih poruka