Good Day ! As per our client aramco , insisting us to do dehydrogenation treatment for P11 material after welding completion for four hours prior to PWHT.

Please clarify whether post heat maintainence for 4hours is mandatory for fillet weld.

As per our WPS  I am doing it for  groove joints , it is clad vessel for 145 inch diameter ... 

Above that insulation and pad welding Accor , is there any clause given in ASME section states that post heat maintainence is not required for P11 material.


As per aramco standard SAESW014 General it is given


P.NEILASHKUMAR 
Sent from my iPad
MOB : 966 551094590
            + 91 9952110791

pgoswami

unread,
Apr 7, 2016, 12:02:30 PM4/7/16
to material...@googlegroups.com

Hi Neilashkumar,

 

There’s no answer to such questions in these “Open Forum”. If such conditions are stipulated in your project specifications, then it’s deemed as mandatory. In order  to get a deviation or any waiver please discuss the same with clients and then come up with some consent/understanding.

 

Many clients insists on “Dehydrogenation” to safeguard against hydrogen induced damages (especially wet hydrogen cracking”) in refining environments. In view of such imminent damage and other forms of hydrogen damages in refining environments, dehydrogenation treatment is most commonly asked for in present day fabrication standards.

 

Thanks.

 

Pradip Goswami, P.Eng,IWE
Independent Welding & Metallurgical Engineering Specialist & Consultant.
Ontario,Canada.
ca.linkedin.com/pub/pradip-goswami/5/985/299

pgos...@quickclic.net

pradip....@gmail.com

 

 


 

 

 

Dear All, 

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0B59ABE0-AA41-4BD5-9389-F1AF70590CAB%40yahoo.com.
For more options, visit https://groups.google.com/d/optout.

Murthy Reddy

unread,
Apr 8, 2016, 12:14:11 AM4/8/16
to material...@googlegroups.com, mur...@indboilers.com

pradip kumar Sil

unread,
Apr 8, 2016, 12:15:38 AM4/8/16
to materials-welding
For P-11 Upto 13mm PWHT is not required also. For P-11 material intermediate stress relief is not required.

Kannayeram Gnanapandithan

unread,
Apr 9, 2016, 12:29:11 AM4/9/16
to materials-welding

If customer requirements, no other way

Vishwas Keskar Welding Manager Pune India

unread,
Apr 18, 2016, 1:26:59 AM4/18/16
to Materials & Welding, jimp...@polarcorp.com
dear sir,

ASME SEC IX OR SEC I , does not give any guidelines for DHT ie post heating.The end user or fabrication company shall decide @DHT based on material , welding joint thickness ,consumable being used (H2 content)
SABIC impose rules when COC are lenient .

Ram Chatt

unread,
Jul 21, 2016, 4:26:23 AM7/21/16
to Materials & Welding, jimp...@polarcorp.com
Hi Mr.Neilash Kumar,

If you are doing Vessel you have to check with API RP-934 A.There is mentioned requirements of dehydrogenation treatment  (post heating).

George Dilintas

unread,
Aug 6, 2016, 6:11:27 AM8/6/16
to Meghanadh K
Preheat Maintenance is a Supplementary Essential Variable for Procedure Qualification. I.e applicable when impact test is required by the Design Code. So if Engineering (ARAMCO) rerquires post heating, you have to make a PQR with post heat maintenance

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis
Reply all
Reply to author
Forward
0 new messages