E7018 Equivalent Filler Wire for SAW

80 views
Skip to first unread message

Thota Kishore

unread,
Sep 22, 2022, 4:56:52 AM9/22/22
to material...@googlegroups.com
Dear Experts,

Could anyone suggest the filler wire & suitable flux for SAW which shall be equivalent to E7018/SMAW.

Thanks in advance.
Regards,
Kishore 

Kannayeram Gnanapandithan

unread,
Sep 22, 2022, 5:15:15 AM9/22/22
to material...@googlegroups.com
F7A2EM12K

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALpPUFsEkoKqSdsHfwdPcTtjY4qGWaD%3DLW3vcyi0c-Yxo7x1%3Dw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages