Dears,
We have one atmospheric hygienic (Food Industry) vertical vessel of SS904L material which is supported on legs. Vessel diameter is 3200 mm & TL-TL is 5100 mm.
The question is, can we weld SS304 directly on SS904L so that we can use SA-312 TP304 pipe l;eg supports?
Is it necessary to have SS904L RF pad instead of SS304?
Can there be an issue with weldability of SS904L with SS304?
Note : - We can’t go for skirt support option.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a8c9b3e-1a20-4200-9d03-cba7a922c1ad%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/409451da-9d6f-4f95-9637-76f23c2fa9eb%40googlegroups.com.
Dear all,
Thanks for your inputs.
This tank we are using for food storage (Extreme Hygienic).
Please tell me what are the issues if we weld SS904L with SS304? SS904L have low carbon while SS304 is having high carbon content.
Will there be any issue of iron contamination in future which may be non-hygienic for food applications?
| From: Makrand Sakpal Sent: Δευτέρα, 30 Μαΐου 2016 - 12:51 To: Materials & Welding Reply To: material...@googlegroups.com Subject: Re: [MW:24907] Re: Problems for SS304 legs on SS904L vessel? |