Dear all,
The Valve material is A182 F347H (i.e. Austenitic stainless steel) and the Pipe nipple used at the hook-up connection between Piping & Instrumentation is Hastelloy C-276
P-Number for A182 F347H is 8 and P-Number for Hastelloy C-276 is 43
Kindly confirm the welding possibility of Authentic Stainless steel with Hastelloy C276.
Regards
Anil
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAN4%2Bm0yLCdzYTR8ne%3DrdBQu3MSSX2Ok9VL0QfA1J1rOX921sDg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
--
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eNxB5o6RNTgL0PeE58huOUH_o9VsuoFjdkcfUaZppBr5w%40mail.gmail.com.