EN 15614-1 Filler material changes & restriction

75 views
Skip to first unread message

Manish Tripathi

unread,
Aug 30, 2022, 3:35:21 AM8/30/22
to Materials & Welding
Dear Members, 
I have doubt that, If WPQR qualified on Group 8.1 with filler ER316L, Can we use to weld by ER308L or ER318 for Group 8.1 material, as per 8.4.4 of EN 15614-1 Level 2. provide all variable remain same.
Regards,
Manish Tripathi

pravin.n...@gmail.com

unread,
Sep 1, 2022, 2:29:44 AM9/1/22
to Materials & Welding
No..

Mohd Siraj

unread,
Sep 1, 2022, 2:30:05 AM9/1/22
to Materials & Welding
No.,ER 316L chemical composition cant be replace by ER308L.

Pravin Kurade

unread,
Sep 1, 2022, 3:02:09 AM9/1/22
to material...@googlegroups.com
No same fillerwire required

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/28325c34-8fe4-4f95-82f9-e83aa98f3650n%40googlegroups.com.
--
Pravinkumar kurade

Kannayeram Gnanapandithan

unread,
Sep 1, 2022, 1:21:12 PM9/1/22
to materials-welding
yes, u can use 318 in place of 316L

--