Specified thickness of the Pipe is 12.7 mm 
Actual thickness measured is 13mm 

Client specified preheating for  12.7 mm (=/>) =75 Deg C

Is preheating is to be decided on specified thickness or  actual thickness?
Any Construction Code back up >


Chris Sabu

unread,
Aug 17, 2020, 12:35:16 AM8/17/20
to material...@googlegroups.com
Preheating is determined by carbon equivalent value.

--


https://materials-welding.blogspot.com/


https://www.linkedin.com/groups/122787


---


You received this message because you are subscribed to the Google Groups "Materials & Welding" group.


To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.


To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/23337554-0c50-46b4-911c-5fdac2322672n%40googlegroups.com.


--
THANKS AND REGARDS
CHRIS SABU
0559695451

Kannayeram Gnanapandithan

unread,
Aug 17, 2020, 2:03:06 AM8/17/20
to materials-welding
specified thickness. ref iso 15614-1

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Kannayeram Gnanapandithan

unread,
Aug 17, 2020, 2:03:07 AM8/17/20
to materials-welding
not only carbon equivalent, thickness, hydrogen level etc. pl ref ISO 1011-2

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

harenath jha

unread,
Aug 18, 2020, 3:36:18 AM8/18/20
to material...@googlegroups.com
As far as designers are concerned they talk about specified thickness.

Sometimes thickness may be  bit more or less then the specified thickness but within the tolerance band. 