Pre-Qualified WPSs

52 views
Skip to first unread message

Zacharias Rohith Joseph

unread,
Jan 9, 2023, 9:59:45 PM1/9/23
to Materials & Welding
While using pre-qualified WPSs is it mandatory to do mechanical tests ? 

If yes , why are they called pre - qualified WPSs then ? 

Thanks 

Faisal Sattar

unread,
Jan 9, 2023, 10:04:18 PM1/9/23
to material...@googlegroups.com
Yes, PWPS means Pre-WPS. Based on that document PQR conducted, that needs mechanical test, root, face bend test and Tensile test. If test results are in acceptance limit than finally PWPS becomes WPS or final document ready for production welding.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bdd9b865-c130-4fb6-a025-01f5ec32f26fn%40googlegroups.com.

Sham Shahabuddin -Welding Inspector, HANBO

unread,
Jan 9, 2023, 10:17:00 PM1/9/23
to material...@googlegroups.com
Dear Mr. Joseph

Unless otherwise you are using the essential variables outside the ranges of pre-qualified WPSs as per the code, there is no need for any tests. 

The ranges of the variables are clearly stated in the code. 

Regards 
Sham Shahabuddin 

--

Kannayeram Gnanapandithan

unread,
Jan 9, 2023, 11:28:31 PM1/9/23
to material...@googlegroups.com
pWPS---prelimary WPS which is to be qualified as per ISO standards
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Jan 10, 2023 at 9:14 AM Kannayeram Gnanapandithan <kgpan...@gmail.com> wrote:
Pre Qualified WPS or Standard WPS need not be qualified, with restrictions u can use.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Kannayeram Gnanapandithan

unread,
Jan 9, 2023, 11:28:35 PM1/9/23
to material...@googlegroups.com
Pre Qualified WPS or Standard WPS need not be qualified, with restrictions u can use.
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Jan 10, 2023 at 8:34 AM Faisal Sattar <faisals...@gmail.com> wrote: