Dears,
I have an bug on EN 15614-1 regarding to pipe description.There is no description of pipe. When I machine below flange from plate, is it designated as pipe or not?

When I have an joint as below,My body material thickness is 50mm. 
My customer requested pipe wpqr for this joint. But I think I can cover this joint with an 30mm Butt Weld WPQR.

What is your opinion?


Kannayeram Gnanapandithan

unread,
Apr 2, 2017, 3:16:51 AM4/2/17
to materials-welding
Which carries Mass and controlled NPS

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b555559d-c5be-4360-8493-9919b3f5b7f7%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Reply all
Reply to author
Forward
0 new messages