Tee connection complete penetration AWS D1.1

20 views
Skip to first unread message

Celestine Emmanuel

unread,
Sep 19, 2016, 10:58:35 PM9/19/16
to material...@googlegroups.com

Dear Experts,
                          As per  AWS D1.1 plate to pipe connection(TC-C) 6G qualified welder can weld this joints,but as per my client view 6GR qualified   welder can only weld this joints, Please give me a clarification as per AWS D1.1. 
 

Thanks in advance,

Celestine Emmanuel

Kannayeram Gnanapandithan

unread,
Sep 20, 2016, 12:36:42 AM9/20/16
to materials-welding
As per table 9.13 of D1.1,  6G welder is eligible to weld  and also 5F welder. There is no requirement for 6GR welder















THANKS & BEST REGARDS,
KG.PANDITHAN, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADTjLvASavpbMwWXzQUzwb4gNFzMZBke0d_APmEZFBqc1uCa_A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Reply all
Reply to author
Forward
0 new messages