Possibility of Crack free in stellite 6 welding?

96 views
Skip to first unread message

Gopalakrishnan G

unread,
May 29, 2019, 12:04:07 PM5/29/19
to material...@googlegroups.com
Dear experts 
 Whether  it is possible to achieve crack free in stellite 6 welding?

I have a job in which I have to carry out hardfacing by stellite 6 and buffer layer with Tenalloy (E-7016).Preheating carried above 350c and interpass 250c with penning and after completion of welding job is covered by heating blanket.
 When I carry out dye penetrant crater cracks appears. But my client needs with 100% crack free.plz kindly give ur valuable guidelines. Thk u.


Regards
G.Gopalakrishnan 
 

Kannayeram Gnanapandithan

unread,
May 30, 2019, 9:15:27 AM5/30/19
to materials-welding
Why are you doing penning? Not 100%. crack free possible if the hardness is more than 35HRC. Why preheat

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKhugu9L6OHAss27tvndZhPOor%2BLHgGcBizCpiHe05O2uA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Gopalakrishnan G

unread,
Jun 1, 2019, 12:58:47 PM6/1/19
to material...@googlegroups.com
Thickness is 90mm and penning for stress relieving ( heat stress)

Kannayeram Gnanapandithan

unread,
Jun 2, 2019, 1:44:17 AM6/2/19
to materials-welding
For stellite peening is not required

Gopalakrishnan G

unread,
Jun 6, 2019, 11:45:26 AM6/6/19
to material...@googlegroups.com
Sir why penning s not required in stellite? 