NEED REFERENCE CODE

42 views
Skip to first unread message

Minhas Arshad

unread,
Oct 11, 2019, 1:42:37 AM10/11/19
to material...@googlegroups.com
Dear Experts,

I would like to ask from all of you that i am working one of the project. I would like to confirm that butt welds with full penetration needs 100 percent radiographic test, is there any reference code? 
I have review the ISO 15614 code table 1 is about examination and testing of the test pieces should i consider this code to QIP.

Regards

Kannayeram Gnanapandithan

unread,
Oct 11, 2019, 5:43:52 AM10/11/19
to materials-welding
what is your construction code/std
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANOHF6tgMyhnE1vxz0iHWpwdynUFasYznL-2t62Smsmw5xpDaw%40mail.gmail.com.

krishnan T

unread,
Oct 11, 2019, 6:58:21 AM10/11/19
to material...@googlegroups.com
Hi. 

It is based on design and may be contact specification requirement.check. 

Aakash

unread,
Oct 21, 2019, 9:36:40 AM10/21/19
to Materials & Welding
Please check your design code and design specification... Otherwise tell us your design code we will explain

Vinay Thattey

unread,
Oct 21, 2019, 9:36:40 AM10/21/19
to material...@googlegroups.com
Dear Minhas

What  is your specification or design requirement ??  You may opt for 100 % , sample , spot or even no RT .. ask your designer .

Reply all