We have pipe line having material API 5L X70 PSL2, dia.8"X 12.7mm, which filler wire for GTAW welding ?
Thanks in advance for your comments. 

Behzad Mohammadi

unread,
Dec 19, 2019, 10:35:06 PM12/19/19
to material...@googlegroups.com
ER 70s

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1a239a49-36b2-452b-931e-d4d57800dd74%40googlegroups.com.

Amitabh Bhattacharya

unread,
Dec 19, 2019, 10:35:11 PM12/19/19
to material...@googlegroups.com
Hi Nilesh

Is the welding carried out in shop or at site ? 

Normally, 8in dia X70 grade can be welded using SMAW process. you may choose E6010 as root welding & Hot, Fill & Cap  using E8018G. Refer  Pipe welding brochure of any reputable maufacturer of filler wire. 

If you go with GTAW ER80B2 may be selected. 
Hope this helps 
Amitabh

Kannayeram Gnanapandithan

unread,
Dec 20, 2019, 10:38:34 AM12/20/19
to materials-welding
In Carbon steel, why do you use Cr-Mo steel consumable. Any specific reasons???

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


Reply all
Reply to author
Forward
0 new messages