What is the Suitable Consumable for CS to Inconel 625 Material for GTAW & SMAW Material.

Process : GTAW & SMAW

Regards,
Manikandan



james gerald

unread,
Feb 23, 2022, 12:16:08 AM2/23/22
to material...@googlegroups.com
ERNiCrMo-3 or ERNiCrMo-10



Inline image
Inline image


Thanks & Regards

J.Gerald Jayakumar




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmNk3ySUGffFw_3pVtosNQj_4AS3S-w9HKS4Bud54qEbDQ%40mail.gmail.com.

George Dilintas

unread,
Feb 23, 2022, 11:06:48 PM2/23/22
to material...@googlegroups.com
What is matching inconel

Manikandan J

unread,
Feb 23, 2022, 11:07:12 PM2/23/22
to material...@googlegroups.com
Dear Sir,

Thanks.Can I use ERNiCRFe-2 as per API RP582?


Reagards,
Manikandan.


james gerald

unread,
Feb 23, 2022, 11:47:15 PM2/23/22
to material...@googlegroups.com
Yes you can. Normally for a higher temperature range and the associated cost.

Inline image

Inline image


Thanks & Regards

J.Gerald Jayakumar


Kannayeram Gnanapandithan

unread,
Feb 28, 2022, 3:33:36 AM2/28/22
to materials-welding
NiCrFe2 for high temp & Creep service.  For ur combination ,it is better to use NiCrMo3
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349