Dear Brothers ,

      I did Pickling and Passivation for SS tank , 

Brand Name : 

1) Pickling : Avesta Pickling Spray 204
2) Passivation : Avesta Finish One Passivator 630

Actually Now i am Facing problem of Molten Slag  Melt at settlement at Shell Plate , Please Refer Attachment file 

My Question Is : If the  Molten Slag not Removed From shell course means ,  will affect any  at Future corrosion  at shell area or Not , According to ASTM A380



Please advice me , I am waiting for your Valuable answer 

Best regards
Sankar.k
Welding Inspector 
Enka-Iraq
20160827_165448.jpg
20160827_165451.jpg
20160828_103337.jpg

Alan Denney

unread,
Aug 28, 2016, 11:52:03 PM8/28/16
to material...@googlegroups.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ed2987e5-5638-49d7-8137-e13a757eb959%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

Shyamal Das

unread,
Aug 29, 2016, 3:21:27 AM8/29/16
to material...@googlegroups.com
Hi

Its better to remove the slag residues .
765

kr
DAS

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.


This email has been scanned by BullGuard antivirus protection.
For more info visit www.bullguard.com

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/000f01d20139%24fadc9750%24f095c5f0%24%40denney1.freeserve.co.uk.
Reply all
Reply to author
Forward
0 new messages