Dear experts,

Greetings of the day

I have a query related to the F Number in welding process.

IF I QUALIFY A WELDER WITH F No.6, He can weld all F.No-6.

But, if I Qualify with F No.5, can he weld F No.1 to 4.

Experts please reply as per code reference.

BEST REGARDS,
NIKHIL THOMAS JOY
IWI LIMITED 
ADNOC-WHRP
0544975526

Dhaneesh p

unread,
Nov 2, 2020, 5:38:40 AM11/2/20
to Materials & Welding
hello 
please follow ASME SEC IX , QW- 433
Regards 
Dhaneesh 

Bhavesh Patil

unread,
Nov 2, 2020, 5:38:45 AM11/2/20
to material...@googlegroups.com
No

He can weld only F No.5 Only refer QW 433

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJxkuiVye%3DvWpXy28w6g%2Bvj77vUNNQHJGZp6dUUi%2Bb5aD1oyOw%40mail.gmail.com.

Kannayeram Gnanapandithan

unread,
Nov 2, 2020, 5:38:49 AM11/2/20
to materials-welding
Ref ASME Sec9 QW- 433. 

On Mon, Nov 2, 2020, 2:30 PM NIKHIL THOMAS JOY <nikhil.t...@gmail.com> wrote:
--

VISHNU DAS BALACHANDRAN

unread,
Nov 2, 2020, 5:38:57 AM11/2/20
to material...@googlegroups.com
Please refer ASME Sec IX, QW-433,
image.png


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJxkuiVye%3DvWpXy28w6g%2Bvj77vUNNQHJGZp6dUUi%2Bb5aD1oyOw%40mail.gmail.com.


--
Regards,

Vishnu Das Balachandran,
PMP®
00965-66983790

*Before printing, think about your ENVIRONMENTAL responsibility!Don't print unless necessary.

senthil vel

unread,
Nov 2, 2020, 10:51:59 PM11/2/20
to material...@googlegroups.com
Dear Sir
As per design the vessel have no PWHT ,
During Repair Preheat Need?


--

Kannayeram Gnanapandithan

unread,
Nov 2, 2020, 11:43:40 PM11/2/20
to materials-welding
Refering code and Thickness 
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


George Dilintas

unread,
Nov 3, 2020, 5:25:20 AM11/3/20
to material...@googlegroups.com
see QW-433 in Section IX
F-no. 5 with backing qualifies only F-No. 5 with backing
F-No. 5 without backing qualifies only F-No. 1 with backing and F-No. 5 with and without backing

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJxkuiVye%3DvWpXy28w6g%2Bvj77vUNNQHJGZp6dUUi%2Bb5aD1oyOw%40mail.gmail.com.


--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

George Dilintas

unread,
Nov 3, 2020, 5:25:24 AM11/3/20
to material...@googlegroups.com
During the repair, you have to implement the same WPS used for production welds..
The depth of the repair may be smaller than the total weld thickness but the PWHT depends on the base metal thickness and not on the deposited metal thickness


Brijesh Maurya

unread,
Nov 5, 2020, 10:34:01 PM11/5/20
to material...@googlegroups.com
F-no. 5 with backing also qualifies F-No.1 with backing along with F-No. 5 with backing as per QW-433

Bien.ND | WIC

unread,
Nov 6, 2020, 7:23:19 AM11/6/20
to Materials & Welding
Agreed this para.