CRA OVERLAY

25 views
Skip to first unread message

Elavarasan Mech

unread,
Jul 16, 2025, 3:44:16 AMJul 16
to material...@googlegroups.com
Dear all 
Please clarify below 
1 . Minimum deposit weld metal thickness 2 mm acceptable as per ASME sec IX &API 6A  corrosion resistance overlay 
2 . Please refer the attached photos for macro examination fusion line waveform acceptable or not for overlay please guide me 

Regards 
ELAVARASAN 