Dear all 
 Please clarify below 
1.5083H116 P NO 
2 . ER 5183 F NO
3.6082 T651
4.ER 5356 F NO

Regards 
Elavarasan 

sridhar cn

unread,
Jun 16, 2025, 7:57:29 AM6/16/25
to material...@googlegroups.com
P Number for 5083-H116: 25
P Number for 6082-T651: 23
F Number for ER 5183:    22
F Number for ER 5356:    22
These classifications are used for qualifying welding procedures and welders. 
C Sridhar. 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ykMv8i956umqUTwE3mCuPXz9qEXbQw0X5eA8FioEs3ScA%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages