As per ASME Section IX, welder qualification for a dissimilar weld (P5A → P8) performed using F-No. 43 filler cannot be done on
P5A → P5A materials alone. The test coupon must include at least one P8 base metal to represent the metallurgical condition of
the production weld. Therefore WQT must be performed on a CS + SS test coupon. CS + CS coupon with F43 is not acceptable under
ASME IX.