Gents,

Fillet welding qualification according to ASME Sec IX 2023
PQR Material - EN 10025-2 S355JR to EN 10025-2 S275JR.

As per QW-424.1, the above materials are listed in the table QW/QB-422 and identified as below
EN 10025-2 S355JR - P-No.1, G.No.2
EN 10025-2 S275JR - P-No.1, G.No.1  

The proposed WPS shall cover one metal from the P-No.1 to any metal from the P-No.1 for the range of qualification.

However referring to ASME Sec IX interpretation record No # 17-3316 (attached), the interpretation seems different for Material SA/EN 10028-2 P355GH. 

Please clarify, if my understanding is correct.

Regards,
Vijay
cstools.asme.org_Interpretation_InterpretationDetail.cfm_TrackingNumber=17019.pdf

Sahil musani

unread,
Mar 8, 2024, 11:44:21 PM3/8/24
to Materials & Welding
Record No # 17-3316 , This interpretation in not valid as on date.
Reply all
Reply to author
Forward
0 new messages