Gas and welding rod compatibility

44 views
Skip to first unread message

Eda Bekar

unread,
Sep 17, 2022, 7:10:42 AM9/17/22
to material...@googlegroups.com
Dear Experts,

The rod and gas we use in our project are СВ08Г2С (russian norm) and M21(%80 Ar + %20 CO2) . We have a lot of porosity and spatter problem. Could you give an advise better than this gas and rod combination?
Materials : C345-5,C255-4,09Г2С-15

Best Regards


furkan topaloğlu

unread,
Sep 18, 2022, 5:06:40 AM9/18/22
to material...@googlegroups.com
Change your consumable şef, everything will be perfect. :)

17 Eyl 2022 Cmt, saat 14:10 tarihinde Eda Bekar <edda...@gmail.com> şunu yazdı:
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/937EC6BF-2A49-4929-8551-B6E4457E1006%40gmail.com.
--

Regards / Saygılarımla

 

Furkan TOPALOĞLU

Metallurgy and Material & Welding Engineer

Metalurji ve Malzeme & Kaynak Mühendisi

Phone : +90 (539) 437 88 03

E-Mail : topalogl...@gmail.com

 

binit kumar

unread,
Sep 20, 2022, 11:25:28 PM9/20/22
to material...@googlegroups.com
Dear Eda,
You can use Э-50А,УОНИИ13/55,РБУ-5,ЦУ-5 rod and kindly check the gas purity.

Regards,
Binit Kumar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/937EC6BF-2A49-4929-8551-B6E4457E1006%40gmail.com.


--
BINIT KUMAR
+918717929495
Reply all
Reply to author
Forward
0 new messages