Technical quary for Electrode E8010 using instead of E7010

47 views
Skip to first unread message

Karunakaran Karan

unread,
Dec 22, 2022, 10:56:44 PM12/22/22
to material...@googlegroups.com
Dear Sir.
   Any have TQ for above subject please share me. My site using E8010 .but Site document mention E7070.so I need TQ for Using E8010.
Thank you

Kannayeram Gnanapandithan

unread,
Dec 22, 2022, 11:21:56 PM12/22/22
to material...@googlegroups.com
usability is same except strength

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw8uFh0UP%2BruTnOPTF7LHjMUWEuzSzeuavfcq%3DOUEHgFTg%40mail.gmail.com.

Karunakaran Karan

unread,
Dec 23, 2022, 4:21:58 AM12/23/22
to material...@googlegroups.com
Dear sir,
          I have one clarification for ELECTRODE QUALIFICATION TEST. OUR PROJECT USING BOTH E6010 AND E8010.PLEASE CLARIFY NEED SEPAPATE TEST FOR E6010 AND E8010 OR ONE TEST FOR BOTH ELECTRODE.PLEASE SIR
   Thanks and regards,

     S.KARUNAKARAN,
      karu...@gmail.com
      91-6382279754
      91-7826930029(Whats app).







MADHUSOODHANAN NAIR .G

unread,
Dec 25, 2022, 10:10:56 PM12/25/22
to material...@googlegroups.com
Definitely both  electrodes required separate EQT.

Regards
M.S NAIR
Mob-7977762694