Unequal wall thickness same base metel

41 views
Skip to first unread message

Karunakaran Karan

unread,
Jan 23, 2023, 10:21:29 PM1/23/23
to material...@googlegroups.com
Dears, 
    Clarify same base metal but different  wall thickness(11.97 and 7.9mm)please any tolerance for fitup and standard.

Karunakaran Karan

unread,
Jan 23, 2023, 10:21:29 PM1/23/23
to material...@googlegroups.com
Asme 31.4 mention 2.38 maimum

Vishwas Keskar

unread,
Jan 24, 2023, 12:37:47 AM1/24/23
to material...@googlegroups.com
Prepare Taper to High Thickness member
Generally  it is 1:4 Taper 

Thanks 
Vishwas —IWE 

Sent from my iPhone

On 24-Jan-2023, at 8:51 AM, Karunakaran Karan <karu...@gmail.com> wrote:


Dears, 
    Clarify same base metal but different  wall thickness(11.97 and 7.9mm)please any tolerance for fitup and standard.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHt4qw8iA06jXxB4BtkBuT9oXtSAZ4%2B7E7zt0vsV6m7U%2Bj0XUw%40mail.gmail.com.
Reply all
Reply to author
Forward
0 new messages