99 views
Skip to first unread message

Vishal Jaiswal

unread,
Nov 15, 2022, 12:26:52 AM11/15/22
to material...@googlegroups.com
Dear Sir,

               Please give information about ER 6010 electrode is need baking or holding in portable oven for the root welding of ERW pipes having thickness range 3 to 8 mm.
Please give suggestions.



Thanks and regards
Vishal kumar
Mechanical Engg.

Bestun Ahmed

unread,
Nov 15, 2022, 3:51:29 AM11/15/22
to material...@googlegroups.com
Hi brother, 
No, no need to hold it or keep it in the oven.

Thanks

Bestoon


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAF6t408Ks6qVdKS5qRuS06scPKDDzchmwsx01G20H3kb7Z71Tg%40mail.gmail.com.

Babur Khan

unread,
Nov 15, 2022, 3:51:34 AM11/15/22
to material...@googlegroups.com
Greetings,
Mr. Vishal, E6010 not require any backing or heating due to cellulosic flux.

Best Regards,

cid:image001.png@01D0FB95.19500D80

Muhammad Babur Khan Lashari
Mechanical Inspector ( Piping / Welding)

Inspection Department
Mob: +966 58 2774568 / 55 968 0573

          +92 334 6186285

Applus Velosi Saudi Arabia

Please consider the environment before printing this e-mail



On Tue, Nov 15, 2022 at 8:26 AM Vishal Jaiswal <vis469j...@gmail.com> wrote:
--

Muhammad Azeem

unread,
Nov 15, 2022, 10:22:46 PM11/15/22
to material...@googlegroups.com
These electrodes are non low hydrogen electrodes which does not required baking before welding , Only need to keep in dry environment and used for downhill welding process. 

Regards,

Muhammad Azeem Iqbal
Welding Inspector Aramco Approved
053110-8577/0554453626/0590071467




Kannayeram Gnanapandithan

unread,
Nov 16, 2022, 10:18:15 PM11/16/22
to materials-welding
6010 doesn't required baking because it is being designed to have more ammount of Hydrogen around 60ml to give better penetration in cross country pipe. Hydrogen is being a non conductivity , it does not allow electric arc to flow smoothly, so more arc force is required to push the current which in tern gives deeper penetration.   IF U DO BAKING, HYDROGEN WILL GET VANISHED

Vishal Jaiswal

unread,
Nov 18, 2022, 3:25:50 AM11/18/22
to material...@googlegroups.com
Dear All,

 Please suggest ,which welding is sutaible for cable tray joint used in PEB Shade.

Ritesh Kumar Singh

unread,
Nov 18, 2022, 3:40:15 AM11/18/22
to material...@googlegroups.com
You can use E 6013 .

On Fri, 18 Nov 2022, 1:55 PM Vishal Jaiswal <vis469j...@gmail.com> wrote:
Dear All,

 Please suggest ,which welding is sutaible for cable tray joint used in PEB Shade.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Vishal Jaiswal

unread,
Nov 18, 2022, 6:07:05 AM11/18/22
to material...@googlegroups.com
Dear all 

What is basic inspection for stud weldind and for welder also

james gerald

unread,
Nov 18, 2022, 6:34:44 AM11/18/22
to material...@googlegroups.com
Check ASME Sec.IX



Inline image



On Friday, 18 November, 2022 at 04:43:16 pm IST, Vishal Jaiswal <vis469j...@gmail.com> wrote:


Dear all 

What is basic inspection for stud weldind and for welder also

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

Vishal Jaiswal

unread,
Nov 20, 2022, 10:48:31 PM11/20/22
to material...@googlegroups.com
Dear All, 

Please suggest wihich welding is sutaible for GI flat bar to GI flat bar  used in cable tray and also which WPS is use for 

Kannayeram Gnanapandithan

unread,
Nov 21, 2022, 1:56:08 AM11/21/22
to material...@googlegroups.com
7018
THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Mon, Nov 21, 2022 at 9:18 AM Vishal Jaiswal <vis469j...@gmail.com> wrote:
Dear All, 

Please suggest wihich welding is sutaible for GI flat bar to GI flat bar  used in cable tray and also which WPS is use for 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.

ahmed adil

unread,
Nov 22, 2022, 3:15:07 AM11/22/22
to material...@googlegroups.com
Dear Vishal

Oxyacetylene welding or Thermit welding are suitable for your job

Best wishes
Ahmed Adil
Welding engineer 

On Mon, 21 Nov 2022, 06:48 Vishal Jaiswal, <vis469j...@gmail.com> wrote:
Dear All, 

Please suggest wihich welding is sutaible for GI flat bar to GI flat bar  used in cable tray and also which WPS is use for 

--

Vishwas Keskar

unread,
Nov 22, 2022, 10:38:33 PM11/22/22
to material...@googlegroups.com
E6010 is best rod for GI trays

Sent from my iPhone

On 22-Nov-2022, at 1:44 PM, ahmed adil <ahmed.a...@gmail.com> wrote:



Gopi Krishna Banerjee

unread,
Nov 23, 2022, 11:10:00 PM11/23/22
to material...@googlegroups.com
SMAW with E 7018 electrode Or  CO2 Welding.

Student

unread,
Jan 16, 2023, 11:30:24 PM1/16/23
to Materials & Welding
6010 is good for galvanized steel. But make sure to clen the joint area of zinc coating before welding, since zinc vapours are health hazard
Reply all
Reply to author
Forward