How to do testing of Reinforced pad

37 views
Skip to first unread message

vinay yadav

unread,
Nov 18, 2016, 9:58:43 PM11/18/16
to Materials & Welding
Dear Sir,

How to do testing of Reinforced Pad. ?

Best Regards,
Vinay.




JIJILAL K M

unread,
Nov 19, 2016, 1:12:26 AM11/19/16
to material...@googlegroups.com
Dear Mr. Vinay,

In API  650 standard  article 7.3.4  it is recommending  for pneumatic pressure test at 100 KPa (1.05 Bar).Once pressure is applied thru tell tale hole, soap solution shall be sprayed to find any leakage.


Best Regards,

JIJILAL K.M. 
QA/QC Manager,
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand



--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8c67ff34-3368-4e41-9b4a-e57167496087%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

dilintas

unread,
Nov 20, 2016, 7:36:20 AM11/20/16
to Meghanadh K
Leak test by blowing into the vent hole. For leak test see Asme V



Sent from my Samsung Galaxy smartphone.

-------- Original message --------
From: vinay yadav <yadav....@gmail.com>
Date: 18/11/2016 09:05 (GMT+02:00)
To: Materials & Welding <material...@googlegroups.com>
Subject: [MW:25729] How to do testing of Reinforced pad

Dear Sir,

How to do testing of Reinforced Pad. ?

Best Regards,
Vinay.




--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.