Dear All, 
Greetings.

WE have manufactured 10% torispherical dish end in house & block dish ends spin hole as per attached photographs. 
Please kindly advise me, is it acceptable as per good engineering practice or not?
Material IS IS2062. Thickness is 10mm. Job - horizontal storage tank


Thanks & Regards,

Rahul Chaudhari
+918149199922
IMG_20211225_141620.jpg
IMG_20211225_141750.jpg

Chiranjeevi A

unread,
Dec 26, 2021, 1:19:38 PM12/26/21
to material...@googlegroups.com
Dear Rahul,

Not acceptable

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjJ0V9Dy0ZrYO60YQkbyXXwHaNkqB8AkXreW-ZM_fc75oqVBA%40mail.gmail.com.

Vishwas Keskar

unread,
Dec 27, 2021, 2:26:28 AM12/27/21
to material...@googlegroups.com
What was joint design?
Is that joint is made full penetration ?
What NDT was followed ?

Pl send details 

--

sushil gaur

unread,
Dec 27, 2021, 2:26:28 AM12/27/21
to material...@googlegroups.com
Hole is accepted as per ASME sec viii. But you have to make "v" On hole and than patch. Also patch should be radiography examination.. 

Thanks & Regards
Sushil Gaur. 