Thicker Plate 4mm SS304L bevel preparation

32 views
Skip to first unread message

mohd helmi

unread,
Oct 16, 2023, 3:22:24 AM10/16/23
to material...@googlegroups.com
Dear Expert,

Please advise bevel preparation for 4mm plate to plate weld, to avoid distortion.Please advise if any procedure can i refer.


Thank you, Regards
Helmi,

  
Reply all
Reply to author
Forward
0 new messages