Impact Testing requirements for PQR

172 Aufrufe
Direkt zur ersten ungelesenen Nachricht

Jackson Raj

ungelesen,
03.05.2023, 01:44:4803.05.23
an material...@googlegroups.com
Dear all,

In Our project has 3 inch to 24 inch and it's thickness 5.49mm to 45.24mm and Impact Testing required for above thickness.
Please clarify how many PQR are required for this job 
Please consider the Impact Testing also mentioned each PQR thickness qualify 

Regards
JJ

Ritesh Kumar Singh

ungelesen,
03.05.2023, 02:01:1403.05.23
an material...@googlegroups.com
3 PQR required as per your job thickness.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALgFOaXAKmJFBKLz39ZoUn%3Dnwi4Er11Qts17%2BbWyQkBOYML4Eg%40mail.gmail.com.
Screenshot_20230503_112635.jpg

Ahmed Osman

ungelesen,
04.05.2023, 06:15:3704.05.23
an material...@googlegroups.com
3 PQR's may be sufficient , 6mm (3-12) 10mm (10-20) 23mm (16-46) 

Best Regards ,
ENG. Ahmed Osman



--

srinivas rao

ungelesen,
04.05.2023, 07:22:1204.05.23
an material...@googlegroups.com
Number of PQR's Required for the project based on BOQ Is depends on below 
 1.construction code 
2. material types involved in scope
3. MDMT of materials 
4. thickness range for each material type
5. applicable client specification requirements 
6 number welding processes you are going to use  
7. scope and due date for delivery/completion of project 
8. Target for daily production based on your capacity if resources.  

If your construction code is B31.3 for normal piping scope and no client specification restriction on dia & thickness range of qualification you need to qualify 4 PQR'S Max with GTAW, SMAW processes , if another process you want to use additional new PQRs to be derived based on thickness. 

Thanks & Regards,
Srinivas Rao 
Welding Engineer 
 



james gerald

ungelesen,
04.05.2023, 07:22:1204.05.23
an 'Ahmed Osman' via Materials & Welding
Appreciate efforts and initiative from ENG.Ahmed.

Just to share. 2 PQR's 6mm & 23mm is sufficient.

There is an ASME Interpretation stating PQR qualified on 6mm and higher thickness qualifies in the range from 16mm.  Someone please share the Interpretation.

Thanks & Regards

J.Gerald Jayakumar




Ahmed Osman

ungelesen,
04.05.2023, 23:18:1204.05.23
an material...@googlegroups.com
Mr. J.Gerald Jayakumar
you mean Interpretation: IX-07-09 ? i think it was mainly asking about splitting of mech. testing , accepted or not ? ( tensile , bend on one PQR and CVN in other one )

Best Regards ,
ENG. Ahmed Osman

james gerald

ungelesen,
04.05.2023, 23:18:1204.05.23
an 'james gerald' via Materials & Welding
ASME B31.3 2018 has the requirements for specimen Thickness BM requirements as per below Snap shot.


Inline image
But in ASME B31.3 BM Thickness requirement for Impact is revised. See below snap shot.

Inline image


Inline image



Thanks & Regards

J.Gerald Jayakumar


Srinivas Rao

ungelesen,
04.05.2023, 23:18:1204.05.23
an Materials & Welding

in addition to above one may consider PWHT requirements if anything applicable as per the design and client spec, if PWHT applicable one may consider additional PQR’s or based on the construction code exemption recommendations PQR's Can be avoided by following pre-heat requirements of the construction code.

Regards, 
Srinivas Rao

james gerald

ungelesen,
04.05.2023, 23:18:1204.05.23
an 'james gerald' via Materials & Welding
ASME Sec.IX Interpretations.

Inline image


Thanks & Regards

J.Gerald Jayakumar


Jackson Raj

ungelesen,
08.05.2023, 09:19:5808.05.23
an material...@googlegroups.com
Dear all

Is it mandatory to do Impact Testing in PQR our clients doesn't approaching to us to do Impact Testing they only required impact Testing in Forging Material Tee and flanges.

That's why we are doing Impact Testing in PQR.

Thanks & Regards
Jack

james gerald

ungelesen,
08.05.2023, 09:52:4608.05.23
an material...@googlegroups.com
Please provide below details

1. MDMT (minimum Design Metal Temperature)
2. Involved Material Grades like ASTM A105 / 106 Gr.B / 333 Gr.6  etc..
3. Applicable design code Like ASME B 31.3
4. Material thicknesses

Thanks & Regards

J.Gerald Jayakumar


Allen antworten
Antwort an Autor
Weiterleiten
0 neue Nachrichten